Starting phase composition is the main driver of hydroxyapatite evolution in apatite-wollastonite glass-ceramics in simulated body fluid, with sintering temperature acting both directly and through the initial phases, and soaking time contributing little.
Initial phase state, not exposure time, governs HA evolution in apatite-wollastonite glass-ceramics
A model-based analysis showing that the starting phase assemblage, shaped by sintering temperature, matters far more than immersion time in determining how hydroxyapatite evolves in SBF.